Abstract
Unlike previous HF etching of Si oxides to produce porous Si a new concept for the preparation of porous SiOx was suggested adopting Si as a pore generating agent and Si oxides as template using NaOH solution. The heat treatment of pristine SiO at 900 C provided nano-crystalline Si within the SiOx matrix. The nano-crystalline Si was dissolved to provide pore size of 200∼500 nm, while most of the SiOx matrix remained as a template during NaOH etching. The surface area of the etched SiO was increased more than 5 times compared with not-etched SiO. The porous SiOx anode exhibited a stable reversible capacity of about 1240 mAh g-1 over 100 cycles at 0.2 C.
Original language | English (US) |
---|---|
Pages (from-to) | 426-430 |
Number of pages | 5 |
Journal | Electrochimica Acta |
Volume | 117 |
DOIs | |
State | Published - Jan 20 2014 |
Externally published | Yes |
Keywords
- Anode
- Lithium batteries
- NaOH etching
- Porous SiO
- Selflate
ASJC Scopus subject areas
- Chemical Engineering(all)
- Electrochemistry