Effect of native oxide mechanical deformation on InP nanoindentation

Research output: Contribution to journalArticlepeer-review

Abstract

Native oxide has been found to have a noticeable effect on the mechanical deformation of InP during nanoindentation. The indentations were performed using spherical diamond tips and the residual impressions were studied by atomic force microscopy. It has been observed that in the early stages of mechanical deformation, plastic flow occurs in the oxide layer while the indium phosphide is still in the elastic regime. The deformed native oxide layer results in a pile-up formation that causes an increase in the contact area between the tip and the surface during the nanoindentation process. This increase in the projected contact area is shown to contribute to the apparent high pressure sustained by the crystal before the onset of plastic deformation. It is also shown that the stress necessary to generate the first dislocations from the crystal surface is ∼3 GPa higher than the stress needed for slip to occur when dislocations are already present in the crystalline structure.

Original languageEnglish (US)
Article number113509
JournalJournal of Applied Physics
Volume104
Issue number11
DOIs
StatePublished - 2008

ASJC Scopus subject areas

  • General Physics and Astronomy

Fingerprint

Dive into the research topics of 'Effect of native oxide mechanical deformation on InP nanoindentation'. Together they form a unique fingerprint.

Cite this