Differential scanning calorimetry of semiconducting As-Se glasses containing Sb

Research output: Contribution to journalArticlepeer-review

Abstract

The compositional dependence of the glass transition temperature (Tg), and the temperature of the maximum rate of crystallization (Tp) of As-Se glasses containing Sb has been measured using non-isothermal DSC. The variation of these characteristic temperatures is found useful in interpreting the structural changes in As-Sb-Se glasses. The role of Sb in these glasses and its effect on the crystallization characteristics is analyzed.

Original languageEnglish (US)
Pages (from-to)107-114
Number of pages8
JournalJournal of Thermal Analysis
Volume32
Issue number1
DOIs
StatePublished - Jan 1987
Externally publishedYes

ASJC Scopus subject areas

  • General Chemistry
  • General Chemical Engineering
  • General Engineering

Fingerprint

Dive into the research topics of 'Differential scanning calorimetry of semiconducting As-Se glasses containing Sb'. Together they form a unique fingerprint.

Cite this